90-Silver 10-Cadmium-Oxide Electrical Contact Alloy

90-silver 10-cadmium-oxide is a precious metal alloy formulated for use in electrical contacts.

The properties of 90-silver 10-cadmium-oxide include three common variations. This page shows summary ranges across all of them. For more specific values, follow the links immediately below. The graph bars on the material properties cards further below compare 90-silver 10-cadmium-oxide to: precious metal electrical contact alloys (top), all alloys in the same category (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elongation at Break

1.1 to 28 %

Shear Strength

170 to 230 MPa 24 to 33 x 103 psi

Tensile Strength: Ultimate (UTS)

260 to 400 MPa 37 to 58 x 103 psi

Other Material Properties

Density

10 g/cm3 640 lb/ft3

Electrical Conductivity: Equal Volume

72 to 100 % IACS

Electrical Conductivity: Equal Weight (Specific)

64 to 91 % IACS

Common Calculations

Strength to Weight: Axial

7.0 to 11 points

Strength to Weight: Bending

8.8 to 12 points

Followup Questions

Further Reading

ASTM B781: Standard Guide for Silver-Cadmium Oxide Contact Material