Annealed 90-Silver 10-Cadmium-Oxide Alloy

Annealed 90-silver 10-cadmium-oxide is 90-silver 10-cadmium-oxide in the annealed condition. It has the lowest strength and highest ductility compared to the other variants of 90-silver 10-cadmium-oxide.

The graph bars on the material properties cards below compare annealed 90-silver 10-cadmium-oxide to: precious metal electrical contact alloys (top), all alloys in the same category (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elongation at Break

28 %

Shear Strength

170 MPa 24 x 103 psi

Tensile Strength: Ultimate (UTS)

260 MPa 37 x 103 psi

Other Material Properties

Density

10 g/cm3 640 lb/ft3

Electrical Conductivity: Equal Volume

100 % IACS

Electrical Conductivity: Equal Weight (Specific)

91 % IACS

Common Calculations

Strength to Weight: Axial

7.0 points

Strength to Weight: Bending

8.8 points

Followup Questions

Further Reading

ASTM B781: Standard Guide for Silver-Cadmium Oxide Contact Material