Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 3.3
76
Elongation at Break, % 20
34
Resilience: Ultimate (Unit Rupture Work), MJ/m3 140
110
Shear Strength, MPa 490
210
Tensile Strength: Ultimate (UTS), MPa 780
320
Tensile Strength: Yield (Proof), MPa 590
300